In this experiment, we used 7-kW continuous wave (CW) CO_(2) low order mode laser and YAG impulse laser to deeply weld high-speed steel (W18Cr4V) and spring steel (65Mn). To welded joint, we analyzed its microstructure, micro hardness and fracture ap